Sell well: Scratch off foil
- Processing Time:
- Shiping out within 3 days
Smarter Shopping, Better Living!
The hot stamping Condition | ||
Ironing | Scalding | |
Temperature Range | 130--170(centigrade) | 180--200(centigrade) |
Stamping’s Head type | Metal | Metal |
Residence time | 1-2s | 10-15/Hour |
Caution: Please reduce the stamping temperature, while it isn’t easy to be scratched off on the cards